Qualifying a new base paper costs a coater far more than the trial reels. Most of the bill is line time, start-up waste, silicone or barrier coating laid on paper you may scrap, lab hours, and the weeks of ageing and customer approval before a single commercial order. The reels themselves are usually the smallest line in the budget.
This article prices that work honestly, for the technical head or procurement manager at a coater, laminator or release-liner producer who has been asked to “just run a trial”. It sets out a trial protocol in stages, the tests at each stage, where the waste comes from, and a worked example you can redo with your own line speed and coat weight. If a term is unfamiliar, the coating base paper glossary defines it.

The cost of qualifying a new base paper is mostly the cost of the coating line not making saleable product. Add the coating chemistry consumed on trial reels, the start-up and calibration waste, lab testing before and after coating, ageing holds, and the commercial risk that the end customer rejects the result after you have paid for all of it.
It helps to split the bill into what you pay in cash and what you pay in capacity. Cash items are visible on an invoice: the trial reels if the supplier charges for them, silicone or barrier coating, catalyst, energy, freight, and any external lab fees. Capacity items never appear on an invoice, which is why they get underestimated. They are the hours a coater spends threading, calibrating and running a material it cannot yet sell, and the slot it could have given to a paying order.
| Cost bucket | What drives it | Cash or capacity |
|---|---|---|
| Trial reels | Number of reels, freight, whether the supplier charges | Cash (often waived) |
| Coating chemistry | Area coated × coat weight, plus extra if the base absorbs more | Cash |
| Start-up and calibration waste | Threading, splices, XRF blank, oven and tension tuning | Cash and capacity |
| Line time | Setup, run, cleaning, and the order that did not run | Capacity |
| Lab testing | Incoming tests, release and anchorage after coating, ageing | Cash (external) or capacity (in-house) |
| Customer approval | Samples converted and run at the customer, weeks of waiting | Capacity and risk |
The last row is the expensive one. A base that passes your tests and fails at the label converter or the pouch maker has cost you the whole trial plus the relationship.
A base paper trial should run in stages that get more expensive as they go, so that a bad base fails early and cheaply. Paperwork and lab tests on a sample come first, then a short coating trial, then full production reels, then conversion and ageing, then customer approval. Each stage should have pass criteria agreed before it starts.
A workable protocol for a release or barrier coater looks like this:
The lab stage cannot be skipped and it cannot be trusted alone. Barry-Wehmiller’s packaging-machinery group, describing its own lab-to-line qualification process, notes that the on-site trial can reveal major issues the lab did not find.
Without pass criteria agreed in advance, a trial produces data and then a meeting argues about what the data means. Write down the release-force window, the maximum rub-off and the acceptable breaks per reel before the first reel is threaded.
The lab tests that belong before coating are the ones that predict how much coating the base will absorb and whether it will run: grammage, caliper, air resistance, surface roughness, water absorptiveness and moisture. They are cheap, they take hours rather than days, and a base that fails them should not cost you line time.
Each has a published test method, and asking for results by method number is the fastest way to find out whether a supplier’s data sheet means anything. Read the results against the incumbents a new base will be priced against, which our glassine, SCK and CCK comparison scores.
| Property | Test method | Why the coater cares |
|---|---|---|
| Grammage | TAPPI T 410 | Sets area per tonne and the reel’s running weight |
| Caliper | TAPPI T 411 | Die-cutting margin downstream, roll diameter, tension response |
| Air resistance (porosity) | TAPPI T 460 (Gurley) | Predicts how much silicone or barrier coating sinks into the sheet |
| Surface roughness | TAPPI T 538 (Sheffield roughness) or a Bendtsen tester | Coating uniformity and coverage at low coat weight |
| Water absorptiveness | TAPPI T 441 (Cobb) | Behaviour under water-based barrier coatings |
| Moisture | TAPPI T 412 | Curl, flatness after the oven, and break risk |
TAPPI T 460 measures the time for 100 mL of air to pass through about 6.45 cm² of sheet at a fixed pressure difference, over a range of 5 to 1,800 seconds, so a higher Gurley reading means a closed sheet. Air resistance is the one to read first. As our explainer on porosity and air permeability in coating base paper sets out, a more open sheet takes more coating to reach the same coverage. That is where most of the hidden cost of a cheaper base turns up.
Measure your current base on the same instruments on the same day. What you need to know is whether the new base is better or worse than the one on your line now, and a side-by-side reading is the only comparison that survives a supplier dispute.
A trial burns coating in proportion to the area coated and the coat weight, and the base decides the coat weight. A more porous base absorbs part of the silicone or barrier layer into the sheet, so the coater has to lay down more to reach the same surface coverage. That extra coating is a cost on every trial metre and, if the base is adopted, on every commercial metre after it.
Most paper release liners run a silicone coat weight of roughly 0.5 to 2 g/m², and where a line sits in that band depends mostly on the base. Momentive’s distributor literature for its SilForce SL6961 solventless system, made for glassine and PE-coated kraft, gives a coat weight of 0.8 to 1.6 g/m². In a technical paper for the Pressure Sensitive Tape Council, Sandra Holtschoppen of Laufenberg sets out the silicone needed for full coverage by base type, with closed glassine at the low end and clay-coated or open bases needing more. A Kammerer patent on primed release papers (US5807781A, 1998) puts the solventless silicone lost into the paper at up to 20 per cent. The more open the base, the further up that band the line has to run to reach coverage. Our piece on silicone holdout, coat weight and anchorage works through that spread in detail.
The arithmetic for a trial is simple enough to do on the back of the trial request:
| Input | Worked example |
|---|---|
| Web width | 1.6 m |
| Line speed | 400 m/min |
| Area coated per hour | 1.6 × 400 × 60 = 38,400 m² |
| Silicone at 1.0 g/m² | 38.4 kg per hour |
| Silicone at 1.3 g/m² (more open base) | 49.9 kg per hour |
| Three trial reels of 10,000 m each | 48,000 m² coated |
| Silicone for the trial at 1.0 / 1.3 g/m² | 48 kg / 62.4 kg |
These are illustrative inputs, not anyone’s line data. Put in your own width, speed and the coat weight you actually need on the new base, and multiply by your own silicone and catalyst price. The figure to watch is the gap between the two coat weights: 14.4 kg on this trial, and on a year of production, the number that decides whether the cheaper base was cheap.
Calibration adds a step that trial plans often forget. Silicone coat weight is measured by energy-dispersive X-ray fluorescence, which FINAT publishes as test method FTM 7. XRF is a relative method, and every base gives off its own background signal, so the uncoated new base needs its own blank and calibration before the coat-weight readings mean anything. Budget the reel length and the lab time for that before the trial starts.

Waste in a production trial comes from threading and start-up, from tuning the oven and tension for a sheet the line has not seen, from splices and breaks, from calibration lengths, and from metres coated before the settings were right. On a short trial these fixed losses can be a large share of everything you run, which is why one-reel trials are so expensive per useful metre.
The fixed losses do not shrink with a shorter trial. Threading, the first splice, the XRF blank and the oven profile cost roughly the same whether you run one reel or five. So a trial long enough to learn something costs little more than the smallest one that keeps the purchase manager happy.
Lighter bases add a specific risk. As our article on running 40-60 GSM paper on a coating line covers, breaks on a light web are usually triggered by tension peaks, edge damage and cross-machine streaks rather than average strength. Øyvind Gregersen’s 2005 review for the Fundamental Research Symposium in Cambridge notes that streaks in caliper, grammage or moisture produce an uneven tension profile across the web, which a single tension readout does not show. A trial on a lighter base needs tension setpoints and every break location logged, or the breaks cannot be explained afterwards.
Log the waste by cause, not as one number:
A trial report that says “1,800 m waste” tells you nothing about the base. A report that says 900 m of that was calibration you would have spent on any new base, and 600 m was two edge breaks, tells you what to ask the supplier.
Enough trial reels means enough to see variation between reels, not just within one. A single reel shows variation within that reel only. Three or more reels, ideally from different production runs at the mill, show you whether the base is consistent, and reel-to-reel consistency is what a converter is actually buying once the trial is over.
Paper standards treat sampling as its own discipline for this reason. TAPPI T 400 sets out how to sample and accept a single lot of paper, and ISO 2859-1 gives sampling schemes indexed by acceptance quality limit for lot-by-lot inspection. Neither tells you how many reels a coating trial needs. They do make the underlying point: a decision about a lot should rest on samples drawn across it, not on whatever came off the top of the truck.
A practical rule for a release or barrier coater is this. If the supplier can only send reels from one production run, treat the trial as a feasibility check, not a qualification, and plan a second trial on reels from a later run before approving the base. The second line slot costs less than finding out in the third commercial delivery that the first trial caught the mill on a good day.
Downtime costs more than the trial reels because a coating line slot is the scarcest thing in a converting business. Every hour spent setting up, running and cleaning down a trial is an hour the line is not producing saleable reels. Unless the line has spare capacity, the real cost of the trial is the margin on the order it displaced.
Plants are bad at pricing this. Valmet, writing on tissue converting, cites an APQC estimate that unplanned downtime costs between 40 cents and $1.20 for every $20 of revenue, and says 80 per cent of plants cannot estimate their downtime accurately. A trial is planned downtime, but the same blind spot applies: nobody costs the slot.
In the worked example above, three reels at 400 m/min take 75 minutes of running. Nobody gets a trial done in 75 minutes. Add threading, the calibration length, oven and tension tuning, at least one splice, sampling stops and the clean-down if the trial uses a different coating system, and a realistic slot is several hours. Each line has its own figure, and that is the one to put in front of whoever is asking for the trial.
Two scheduling habits cut this cost without cutting the trial. Run the trial at the end of a production run on the same silicone or barrier system, so there is no extra changeover and clean-down. And run trials for several candidate bases in one slot if you have them, because the fixed set-up cost is then shared across them.
Weekend or short-staffed shifts are a false economy. A trial run when the senior operator is off produces breaks nobody can explain, and an unexplained break is a reason to run the trial again.

A full base paper qualification usually takes weeks to months, and most of that time is waiting rather than running. Lab tests take days, the coating trial takes a shift, but accelerated and real-time ageing, conversion at the customer, and the customer’s own approval cycle take much longer. Build the calendar before the trial, not after.
Ageing is the stage most often underestimated. Anchorage that passes on the day of coating can fail after storage, which is why release coaters age samples before signing off. A Dow Silicones patent (US10023767B2, 2018) describes ageing samples for 10 days at room temperature and for 7 days at 70 °C and 90 per cent relative humidity, then measuring rub-off by XRF before and after abrasion. Release force is then tested at low and high peel speeds under FINAT FTM 3 and FTM 4, and the label’s subsequent adhesion under FTM 11. FTM 10, FINAT’s release-force method for silicone-coated substrates, conditions 25 mm strips for 20 hours under load at 23 °C before a 180° peel at 300 mm/min, with an optional 20 hours at 70 °C as accelerated ageing. An International Paper patent on universal release-liner papers (US8455076B2, 2013) uses the same two checks this protocol leans on: rub-off for anchorage and solvent extraction for degree of cure.
Food-contact work can add its own wait. Regulation 4(1)(c) requires paper in contact with food to be food grade and free from contaminants. Under the Food Safety and Standards (Packaging) Regulations, 2018, Regulation 4(4)(b) requires packaging materials of plastic origin to pass an overall migration limit of 60 mg/kg or 10 mg/dm² when tested to IS 9845. A paper whose food-contact layer is a plastic coating falls under that test. Our guide to food-contact compliance for coated paper in India covers which layer the rule applies to.
An indicative calendar for a release-liner base looks like this:
| Stage | Typical duration | What you are waiting for |
|---|---|---|
| Paperwork and sample tests | 1-2 weeks | Sample arrival, lab queue |
| Short coating trial | 1 shift | A line slot on the right coating system |
| Production trial reels | 1-2 weeks | Reels from the mill, a scheduled slot |
| Post-coating and ageing tests | 1-3 weeks | Accelerated and room-temperature ageing |
| Customer conversion and approval | Several weeks | The customer’s own trial and sign-off |
The durations are planning ranges, not measured figures; your own customers set the last row. What the table shows is that the line work is a small part of the calendar.
You cut the cost of a base paper trial by failing bad candidates early, sharing fixed set-up costs and agreeing pass criteria before anything is coated. Each of these removes spending that tells you nothing about the base, and none of them shortens the tests.
A checklist to send with every trial request:
Everything above applies with extra force to a base that is still in development, because there is no production history to lean on. Pakka’s coating base paper programme, flexC base, is in that position, and a converter weighing it should read the limitations first.
flexC base has no published performance specification yet. There is no porosity, roughness, Cobb or release data to compare on paper, so a converter would be qualifying it from the first stage of the protocol above, not checking a data sheet. It is also lighter than the standard glassine release band, which means the runnability points in this article apply in full. Porosity is one of the properties you would need to measure on your own instruments rather than take on trust.
What is disclosed is this. flexC base is a coating base paper in the 40-60 GSM band, made bleached and unbleached, intended as a substrate for silicone, biopolymer and plastic barrier chemistries. The company has named eight target applications: confectionery wraps, snack pouches, sachets, medical packaging, seed packs, release liners, dry food liners and tea pouches. These details come from Pakka Limited’s Investor Presentation for Q1 FY2026-27, filed on 18 August 2026 (BSE 516030 / NSE PAKKA).
flexC base is not flexC. flexC is Pakka’s finished compostable flexible-packaging laminate, a separate product sold to brand owners; flexC base is the uncoated paper a coater would put its own chemistry on.
For a coater, the case is narrow. If you are already planning to qualify a lighter or alternative base, a development programme lets you agree test methods and pass criteria with the mill while the specification is still being set. Every stage of the trial above would still apply.
At least three, and ideally from different production runs at the mill. One reel shows within-reel variation only. Reel-to-reel consistency is what you are buying, so a trial on reels from a single run should be treated as a feasibility check and followed by a second trial.
Grammage (TAPPI T 410), caliper (T 411), air resistance by Gurley (T 460), Sheffield roughness (T 538) or Bendtsen, Cobb (T 441) and moisture (T 412). Measure your current base on the same instruments on the same day for comparison.
Because a more porous base absorbs part of the coating, so you need a higher coat weight to reach the same coverage. At 400 m/min on a 1.6 m web, moving from 1.0 to 1.3 g/m² adds about 11.5 kg of silicone an hour. Over a year that can outweigh the saving on the paper.
Usually several weeks to a few months. The coating trial is one shift, but accelerated ageing, customer conversion and the customer’s own approval take most of the time. A Dow patent describes ageing release samples for 7 days at 70 °C and 10 days at room temperature before testing.
Under FSSAI’s Packaging Regulations, 2018, migration testing to IS 9845 is mandatory for packaging materials of plastic origin. If the food-contact layer of your coated paper is a plastic, a base change is a good reason to retest the finished structure.
Last reviewed: November 2026
Planning a base paper trial? If you are qualifying a lighter or alternative coating base and want to agree test methods and pass criteria before the first reel, send us a flexC base trial enquiry with your coating system, line width and speed, current base grade and the converters or brand owners your material goes to. Technical brochures for our paper and packaging range are on the resources page, and general enquiries reach us through the same contact page.
Browse all Pakka articles.